Coagulation is the quiet workhorse of water treatment: it removes suspended solids and colloidal particles that do not settle naturally, reduces turbidity, and even partially removes bacteria and viruses. The mechanism splits into perikinetic flocculation, caused by Brownian motion, and orthokinetic flocculation, caused by external fluid movement. But knowing the mechanism does not pick your chemical. For that, the properties of each coagulant — and their field quirks — decide the answer.

The Operating Rules Before the Chemical Choice

A few dosing rules frame everything that follows. The common iron and aluminum salts are dosed in a range of 10-100 mg/L. When inorganic flocculants are used together with organic flocculants, the inorganic coagulant should be dosed first, followed by the organic flocculant. The factors affecting coagulation performance include water temperature and pH value — and as the next sections show, temperature and pH are exactly where each chemical shows its personality.

Aluminum Sulfate: The Workhorse With a Temperature Problem

Aluminum sulfate contains varying amounts of water of crystallization, written Al2(SO4)3·nH2O, where n = 6, 10, 14, 16, 8 and 27; the commonly used form is Al2(SO4)3·18H2O, with a molecular weight of 666.41 and a specific gravity of 1.61, appearing as white, glossy crystals. It is readily soluble in water, its aqueous solution is acidic, solubility at room temperature is about 50% with a pH below 2.5, and in boiling water solubility rises above 90%. In operation it is convenient to use and gives good coagulation without adversely affecting the treated water quality — the reason it remains a default choice.

Its weakness is cold water. When the water temperature is low, hydrolysis of aluminum sulfate is difficult and the flocs formed are loose. Overdosing brings a second trap: adding excess aluminum sulfate can lower the water pH below the range effective for aluminum-salt coagulation, wasting chemicals and impairing the quality of the treated water at the same time.

Ferric Chloride: Strong, but Hungry for Corrosion-Resistant Hardware

Ferric chloride (FeCl3·6H2O) is a commonly used coagulant — a dark brown crystal with strong hygroscopicity, highly soluble in water, its solubility increasing with temperature. The floc it forms settles well, and it performs better than aluminum salts for treating low-temperature or low-turbidity water, which makes it the natural answer where aluminum sulfate struggles.

The supply forms matter: in China it comes in anhydrous, hydrated (crystalline) and liquid forms, and the liquid, crystalline, or moisture-exposed anhydrous forms are all highly corrosive. Chemical preparation and dosing equipment must use corrosion-resistant materials — stainless steel pump shafts corrode within weeks, while titanium pump shafts offer much better corrosion resistance. Chemically, after ferric chloride is added to water it reacts with the alkalinity in natural water to form ferric hydroxide colloid. The advantages are a floc with high specific gravity that settles easily, good performance at low temperature and low turbidity, and a fairly wide suitable pH range. The drawbacks are the strongly corrosive solution and a higher color of the treated water than with aluminum salts.

Ferrous Sulfate: Cheap, But Watch the Color

Ferrous sulfate (FeSO4·7H2O) is a translucent green crystal, commonly known as green vitriol, dissolving easily in water with a solubility of 21% at 20°C. It is usually a by-product of manufacturing other chemical products and is inexpensive, but its heavy metal content should be tested to ensure that, at the maximum dosage, the heavy metal levels in the treated water do not exceed the limits set by the relevant national water quality standards. Solid ferrous sulfate must be dissolved before dosing, generally prepared as an approximately 10% solution by weight.

Two color-related traps demand attention. The Fe2+ remaining in the water will increase the color of the treated water, and when the water has a high color value, Fe2+ reacts with the colored substances, producing darker substances that are difficult to settle.

Oxidation is the fix, and the water chemistry dictates the route. When the water pH is above 8.0, the Fe2+ of the added ferrous salt is easily oxidized by dissolved oxygen in the water to Fe3+. When the raw water pH is low, ferrous sulfate can be used together with alkaline chemicals such as lime and activated silica — activated under alkaline conditions — to promote the oxidation of ferrous iron. When the raw water pH is low and dissolved oxygen is insufficient, ferrous iron can be oxidized by chlorination:

6FeSO4+3Cl2=2Fe(SO4)3+2FeCl3

According to this reaction equation, the theoretical dosage ratio of ferrous sulfate to chlorine is about 8:1, but in actual practice, to ensure rapid and complete oxidation of ferrous iron, the chlorine dosage can be slightly increased as appropriate. When there is not enough dissolved oxygen in the water, chlorine or bleaching powder can be added for oxidation; theoretically, 1 mg/L of FeSO4 requires 0.234 mg/L of chlorine.

Lime Calculations and the pH Window

When the water pH is below 8.0, lime can be added to remove CO2 from the water, with the lime dosage estimated by the formula [CaO]=0.37a+1.27CO2 (1.18), where a is the FeSO4 dosage (mg/L) and CO2 is the CO2 content in the water (mg/L). When iron salts are used, the applicable pH range of the water is wide, between 5.0 and 11 — a flexibility that partly compensates for their corrosion and color issues.

The Magnesium Carbonate Footnote

Magnesium carbonate deserves a mention alongside the big three. It forms an Mg(OH)2 colloid in water similar to the Al(OH)3 and Fe(OH)3 colloids produced by aluminum and iron salts, and can clarify water. In the sludge of lime-soda water softening plants, besides calcium carbonate, there is also magnesium hydroxide; carbon dioxide gas can dissolve the magnesium hydroxide in the sludge, thereby recovering magnesium carbonate.

What Happens to the Sludge

Whatever chemical is chosen, the aluminum and iron salts added as coagulants form flocs that settle together with the impurities and become sludge that must be properly treated to avoid pollution. Large water plants produce large amounts of sludge, so many have tried recovering the effective aluminum and iron from the sludge with sulfuric acid — but the recovered material often contains large amounts of iron, manganese and organic color, making it unsuitable for reuse as a coagulant. Coagulant selection, in other words, is not just a dosing decision; it is a lifecycle decision spanning corrosion, color, sludge and cost.